Ubuso obugandayiwe obunombala · Umhlahlandlela wokusetshenziswa ongokoqobo
Izingxenye zikakhonkolo zokugandaya ezinombala. Izivivinyo zengxube yobuso.
Bala umbala oyimpuphu kuphela ngongqimba olufanele olunombala, bese ugunyaza kokubili izingxenye zokugandaya ngayinye nokusatshalaliswa kwemibala uma sezibekiwe.

Hlonza ungqimba oludinga umbala oyimpuphu
Ingxenye kakhonkolo yokugandaya ingafakwa umbala kuyo yonke indawo noma ibe nongqimba lobuso olunombala olukhiqizwa ngokwehlukana. Thola ingxenye enqamulelayo yangempela yomkhiqizo neshidi lenqwaba. Umbala oyimpuphu wengxube yobuso ubalwa ngesisekelo esichaziwe sento ebophayo saleyo ngxube yobuso, hhayi ngokuzenzakalelayo ngokusebenzisa usimende wongqimba olungemuva. Ukujiya okudingekayo kobuso nokusebenza komkhiqizo kuhlala kuyingxenye yedizayini ekhona.
Sebenzisa inkomba yokuqala eqondene nokusetshenziswa
Ishidi le-MAPEI le-Color Paving Pigment linikeza 3–6% ngokwesisindo sikasimende uma kusetshenziswa usimende ompunga, kanye no- 1–4% uma kusetshenziswa usimende omhlophe ebangeni lemikhiqizo yalo. Lezi yizinkomba zemikhiqizo eqanjwe amagama zokukhetha amazinga ezivivinyo, akuzona iziqinisekiso zemithamo ye-FUXIN. Liphinde liveze ukuthi ukwengeza umbala oyimpuphu ngokwengeziwe kugcina kunikeza umbala owengeziwe omncane kuphela. Iziqondiso zemithamo yokugandaya kukakhonkolo
Ngengxube yobuso bukasimende ompunga eno 20 kg usimende, ukuqhathanisa kokuqala okugunyazwe umphakeli ku-3%, 4% no-5% kungadinga:
| Isampula yengxube yobuso | Umbala oyimpuphu / usimende | Impushana eyomile |
|---|---|---|
| Isampula lokuqhathanisa | 0% | 0 g |
| A | 3% | 600 g |
| B | 4% | 800 g |
| C | 5% | 1,000 g |
Gcina isihlabathi, amanzi nezithasiselo kungashintshi kulokhu kuqhathanisa. Uma umkhiqizo esikhundleni salokho uchaza isisindo esiphelele sezinto zikasimende njengesisekelo sawo, bala kabusha ngokufanele. Ibanga lombala oyimpuphu elikhethiwe nefomula ephelele yengxenye yokugandaya kunquma ukuthi yimaphi amazinga angahlolwa.
Gwema iphutha lokubala amanani ongqimba lobuso
Ake sithi isabelo sokukhiqiza siqukethe 20 kg kasimende wongqimba lobuso kanye no-40 kg kasimende wongqimba olungemuva. Ngomthamo okhethiwe ongu-4% kasimende wobuso, umbala oyimpuphu ungu- 0.8 kg. Ukubala u-4% wawo wonke u-60 kg kuzonikeza u-2.4 kg, okuyizikhathi ezintathu zokwengezwa okuhlosiwe kwengxube yobuso.
Gcina amarekhodi obuso nawengemuva ehlukene ngisho noma isilawuli esisodwa sokukhiqiza silawula womabili. Ungongi umbala oyimpuphu ngokwenza ungqimba lobuso oluncane ngokujiya olungagunyaziwe. Lokho kushintsha umkhiqizo kunombala wawo kuphela. Ngombala ofinyelela kubo bonke ubukhulu, sebenzisa into ebophayo egunyaziwe eyisisekelo sokubala yengxube ephelele enombala bese uhlola isampula kabusha.
Yenza isivivinyo sokucindezela noma sokuthela esibunjeni
- Hlola ukulinganiswa kombala oyimpuphu nomswakama wezihlanganisi. Hlonza amaqoqo angenayo kasimende nawombala oyimpuphu.
- Sebenzisa ukulandelana okuqinisekisiwe kokufaka izinto nezinga lokugcwaliswa komshini wokuxuba. Hlola ingxube esatshalaliswe ebusweni noma isampula ecindezelwe ukuze ubone ukusatshalaliswa ngaphambi kokucabanga ukuthi umbala oyimpuphu owengeziwe uyadingeka.
- Bumba ngemishini yokukhiqiza, ubhale izilungiselelo zokudlidliza, ukucindezela nokuphakela ungqimba lobuso. Iziqondiso ze-Davis zokukhiqiza zihlonza lokhu njengezinto eziguqukayo ezithinta ukubukeka kobuso. Ukulawula inqubo yezingxenye ezikhiqiziwe
- Maka amasampula ezindawo ezahlukene zokukhiqiza nendawo yokuvuthwa. Qedela indlela evamile yokuvuthwa, ukuqedela ubuso nokupakisha.
- Qhathanisa izingxenye ezomile ngaphansi kokukhanya okufanayo, bese uqedela ukuhlolwa okudingekayo kobukhulu, amandla, ukuguga nokuchayeka ezimweni. Gcina leyo miphumela eceleni kokugunyazwa kokubukeka.
Gunyaza inhlanganisela ebekiwe, hhayi ingxenye eyodwa ekhangayo yokugandaya
Ngohlelo lwemibala emibili oluphakanyisiwe oluno 70% umbala A no-30% umbala B, isampula yamayunithi ayi-100 idinga amayunithi angu-70 e-A namayunithi angu-30 e-B. Lesi yisibonelo sokusatshalaliswa komklamo, hhayi ingxube ye-pigment ngaphakathi komxubi. Kubeke ngokwephethini ehlosiwe nendlela yokusabalalisa. Inqwaba yamayunithi anombala ofanele isengadala ukufakwa okunemigqa okungafuneki.
Bhala inhlanganisela eyamukelwe ngesithombe nokuhlonzwa kwezingxenye. Hlola umbukiso womile futhi umanzi. Gcina amasampula okushintsha ombala ngamunye oyingxenye yenhlanganisela ukuze ama-oda akamuva afaniswe namafomula awo ngamanye.
Xazulula izinkinga zobuso obubonakalayo
| Ukubukeka | Hlola kuqala |
|---|---|
| Ukufiphala okukhanyayo | Okunqwabelene nomlando womswakama |
| Imigqa emile ekuhlelweni | Ukusatshalaliswa kwezingxenye nokuhlanganiswa ngamaqoqo ezinqwaba |
| Izingxenye ezimahhadlahhadla zibukeka zimnyama kakhudlwana | Ukucindezela nokuthungwa kobuso |
| Umbala uyashintsha ngemva kokuguga | Ukuvezwa kwezihlanganisi nokulahleka kwengxube ewugqinsi kasimende |
| Inqwaba eyodwa ayihambisani nethoni | Amarekhodi okukala ngesisindo, into ebophayo namanzi |
Iziqondiso ze-CMHA zokunakekelwa zihlukanisa ukuphuma kukasawoti ebusweni nokushintsha kobuso ekufiphaleni kombala oyimpuphu. Ukubukeka nokunakekelwa kwezingxenye zokugandaya Hlola noma iyiphi into yokuhlanza noma evalayo ezingxenyeni ezigciniwe. Thumela kwa-FUXIN indlela yobuso/yobukhulu bonke, isisekelo sikasimende, isampula eyomile efunwayo nemiphumela yokukhiqiza lapho ucela ibanga lombala oyimpuphu.
Izithenjwa zobuchwepheshe
- MAPEI: I-Color Paving Pigment
- Davis Colors: Ukukhiqiza izingxenye zikakhonkolo ezinombala
- CMHA: Ukunakekelwa kobuso obugandayiwe ngezingxenye ezikhiyelanayo
Kusetshenziswe iziqondiso zobuchwepheshe ezizimele kulokhu kuhlolojikelele kokusetshenziswa. Lezi zinkomba azizona izifundo zamaphrojekthi e-FUXIN noma indawo yeshidi ledatha yobuchwepheshe eliqondene nebanga lomkhiqizo.