Ukugandaywa okusekelwe esihlabathini okuvumela amanzi adlule · Umhlahlandlela wokusetshenziswa ongokoqobo
Ukugandaywa okusekelwe esihlabathini. Ukuhlolwa kombala nokugeleza kwamanzi.
Gcina into yokufaka umbala ngaphakathi kwefomula egunyaziwe yesihlabathi nento ebophayo bese ukala ukugeleza kwamanzi ngaphandle kokuphambanisa isampula yombala nesitifiketi sokukhipha amanzi.

Hlonza into ebophayo nendlela yamanzi
Imikhiqizo esekelwe esihlabathini evumela amanzi adlule ingasebenzisa isihlabathi esigcotshwe nge-resin, izinto zikasimende noma inhlanganisela yezingqimba ezahlukene. Thola ingxenye enqamulelayo yangempela nokuthi ngubani ongumnikazi wefomula ngaphambi kokukhetha umbala oyimpuphu. Nquma ukuthi amanzi adlula engxenyeni, ezikhaleni noma kuzo zombili. Udaka oluvamile oluminyene nobuso obuvumela amanzi adlule obunefomula yomkhiqizi abukwazi ukwabelana ngeresiphi yombala ecatshangelwayo.
Ucwaningo lokuqala lwezitini eziyinhlanganisela yezinto ezivumela amanzi adlule luhlanganisa ubuso be-resin nesihlabathi nesisekelo sezinto zikasimende futhi lubika ukulinganisa phakathi kokushintsha kwefomula nokuziphatha ngokomzimba. Aluqinisekisi umthamo ovunyelwe wombala oyimpuphu komunye umkhiqizo. Ucwaningo lwezitini eziyinhlanganisela yezinto
Bala ngokwesisekelo esichaziwe songqimba olugunyaziwe
Alikho iphesenti elilodwa le-iron oxide elisebenza kuzo zonke izimo kulesi sigaba. Sebenzisa kuphela umthamo ogunyaziwe wento ebophayo yangempela. Isibonelo esilandelayo esicatshangelwayo esingu-1% sibonisa umehluko phakathi kwezisekelo zokubala ezingaba khona; akuyona iresiphi noma ukugxila okunconyiwe.
| Isisekelo esibhalwe phansi kufomula ecatshangelwayo | Inani lokubhekisela | Into yokufaka umbala ongu-1% |
|---|---|---|
| Into ebophayo ye-resin kuphela | 0.50 kg | 5 g |
| Isisindo sesihlabathi | 10.00 kg | 100 g |
| Usimende ongqimbeni oluhlukile lwezinto zikasimende olugunyaziwe | 2.00 kg | 20 g |
Ukubala ngokusebenzisa isihlabathi esikhundleni se-resin echaziwe engu-0.50 kg kuzonikeza okuphindwe ngamashumi amabili kombala oyimpuphu ohlosiwe. Isibonelo songqimba lukasimende singenye ifomula, akusona esinye indlela yokulinganisa umthamo walobo buso obufanayo. Gcina isilinganiso sezithako sanoma iyiphi into ebophayo esabelayo singashintshi bese uthola imvume yokwakheka kwamakhemikhali ombala oyimpuphu nokuqukethwe kwawo komswakama.
Yenza amasampula ahamba ngambili ngaphandle kokushintsha ukwakheka kwezimbotshana
- Sebenzisa isampula yokuqhathanisa engenambala nomthamo ogunyaziwe ozohlolwa. Bhala ukumiswa kosayizi besihlabathi, iqoqo lento ebophayo, isisindo sangempela sombala oyimpuphu nesimo somswakama.
- Satshalalisa umbala ngendlela egunyaziwe yomsunguli. Ungafaki into ebophayo eyengeziwe ngenxa nje yokuthi ingxube efakwe umbala oyimpuphu izwakala ihlukile; lokho kungashintsha into yesibili eguqukayo.
- Bumba amasampula alinganayo ngokujiya, umfutho noma ukucindezela nendlela yokuvuthwa okufanayo. Hlonza izingqimba ngokwehlukana engxenyeni yenhlanganisela yezinto.
- Hlola izigaxa zombala oyimpuphu, ukugcotshwa okungalingani nokuvala kobuso okubonakalayo. Gcina ingxenye yeqoqo lamasampula yomile ukuze kuqhathaniswe umbala.
- Hlola izici ezichaziwe ze-mechanical nezokugeleza kwamanzi ngelabhorethri yomkhiqizo. Ubuso obubukeka bukhangayo obulahlekelwa amandla adingekayo okudlulisa amanzi abuwona umphumela wombala owamukelekayo.
Sebenzisa izibalo ezilula zokugeleza njengerekhodi lokuqhathanisa kuphela
Ilabhorethri ingaqhathanisa ivolumu eqoqiwe ngesikhathi esingashintshi, igcine indawo yesampula, ukujiya, ukuphakama kwekholomu yamanzi nokulungiswa kwezimo kungashintshi. Isilinganiso sokugeleza Q = ivolumu eqoqiwe / isikhathi.
Ekubhekeni okucatshangelwayo kwamasampula ahamba ngambili, isampula yokuqhathanisa idlulisa u-900 mL ngemizuzu engu-10 nesampula efakwe umbala oyimpuphu idlulisa u-800 mL ngemizuzu engu-10. Izilinganiso ezihambisana nalokho zingu- 90 no-80 mL/min; ukugeleza kwesampula ezohlolwa/kwesampula yokuqhathanisa kungu- 88.9%. Lezi zibalo azilona inani le-coefficient yokudlula kwamanzi, umphumela wesivivinyo esimisiwe noma umkhawulo owamukelekayo. Indlela nezimfuneko zephrojekthi kufanele zinqume ukuthi izinto ziyaphumelela yini ekuhlolweni.
| Bhala phansi | Gcina kufana noma ubhale phansi |
|---|---|
| Isimo sejiyomethri sesampula | Indawo, ukujiya nokuhlelwa kwezingqimba |
| Ukulungiswa kwezimo | Ubudala bokuvuthwa, umswakama nezinga lokushisa |
| Ukuhlelwa kokuhlola amanzi | Ukuphakama kwekholomu yamanzi, indlela yokuhlinzeka neyokuqoqa |
| Ukugeleza okubonwe | Ivolumu nesikhathi esidlulile |
| Ukubukeka | Ubuso obomile, obumanzisiwe nobuphinde bomiswa |
Hlola ukunakekelwa nokushintsha kobuso
Ungafafazi umbala oyimpuphu ebusweni obuqediwe obuvumela amanzi adlule noma ufake into evalayo ukuze uthuthukise umbala kuphela. Kokubili kwethula ukushintsha kobuso okungalawulwayo. Hlola izinqubo ezigunyaziwe zomsunguli ngokuphathelene nezinsalela ezizinze phansi nokunakekelwa kulo lonke uhlelo. Iziqondiso ze-CMHA zokugandaywa okuvumela amanzi adlule zichaza ukulahleka kokungena kwamanzi okubangelwa yizinsalela ezingxenyeni zokugandaya ezikhipha amanzi ngezikhala, okuwuhlelo oluhlukile imininingwane yalo okungafanele idluliselwe engxenyeni ye-resin nesihlabathi. Umongo wokunakekelwa nokuhlukaniswa kwezinhlelo
| Okutholakele | Uphenyo olulandelayo |
|---|---|
| Ukugeleza kuyehla ngemva kokufaka umbala oyimpuphu | Ukusatshalaliswa, ungqimba lwento ebophayo nokubumba |
| Okumhlophe noma okunombala okukhukhulwa ngamanzi | Ubuqotho bobuso nokuphuma kwezinto |
| Izingqimba zento eyinhlanganisela ziyahlukana | Ukuhambisana komngcele wokuhlangana nokuvuthwa |
| Umbala ushintsha kuphela lapho kumanzi | Qhathanisa ngemva kokomisa kabusha ngokulinganayo |
Gcina ndawonye imiphumela yombala, ukugeleza namandla. Thumela kwa-FUXIN ukwakheka kwamakhemikhali ento ebophayo, isisekelo somthamo esigunyaziwe nemiphumela yamasampula ahamba ngambili. Ungaguquli lezi zivivinyo zibe izimangalo zokuhlanza amanzi, ukuziphatha okungavimbi unomphela noma ukufaneleka kwezemvelo ngaphandle kobufakazi obufanele bomkhiqizo oqediwe.
Izithenjwa zobuchwepheshe
- Wang, Liu no-Mei: Ucwaningo lokuqala lwezitini eziyinhlanganisela yezinto ezivumela amanzi adlule
- Ucwaningo lokuqala: Izitini ezisekelwe esihlabathini se-silica ezivumela amanzi adlule
- CMHA: Ukunakekelwa kobuso obugandayiwe ngezingxenye ezikhiyelanayo ezivumela amanzi adlule
Kusetshenziswe iziqondiso zobuchwepheshe ezizimele kulokhu kuhlolojikelele kokusetshenziswa. Lezi zinkomba azizona izifundo zamaphrojekthi e-FUXIN noma indawo yeshidi ledatha yobuchwepheshe eliqondene nebanga lomkhiqizo.