Paints and coatings · Practical application guide
Paints & coatings. Dispersion trials.
Calculate colorant and dispersant separately, run an identifiable millbase trial, and compare the finished paint rather than the wet pigment paste.

First separate three different percentages
A paint formula can state dry pigment as a percentage of finished paint, pigment concentration in a paste, or dispersant addition on pigment. These are different denominators. Write the basis next to every figure before weighing. Keep the binder, pigment chemistry, surface treatment, waterborne/solventborne route and required film finish identified. A color name does not establish that a green, blue or purple product is an iron oxide.
Use the existing approved paint formulation to select the final colorant loading. The practical window below concerns a named dispersant in a water-only pigment concentrate; it is not a universal iron-oxide dose or a solventborne paint recipe.
A sourced dispersant ladder you can calculate
BYK’s DISPERBYK-190 coating TDS gives 20–30% additive as supplied, based on inorganic pigment mass, and typical nonvolatile matter of 40%. Titanium dioxide has a separate dosage entry; do not apply this inorganic-color-pigment window to it. The 40% is nonvolatile matter, not a certified active-content assay. This additive requires grinding in water without binder, amines or cosolvents; confirm compatibility before using that route. BYK dosage and incorporation instructions
For a screening charge containing 200 g dry inorganic pigment, the calculations are below. The pigment charge is a convenient calculation size, not a specified total millbase concentration. The middle point is an interpolated trial within the published range.
| Trial | Additive/pigment | Additive as supplied | Typical additive nonvolatile matter |
|---|---|---|---|
| A | 20% | 40 g | 16 g |
| B | 25% | 50 g | 20 g |
| C | 30% | 60 g | 24 g |
Calculated as pigment mass × addition fraction; additive solids = supplied mass × 0.40. Preserve the chosen grind’s workable solids and liquid balance when setting its water quantity. Record the balance explicitly. Do not confuse the nominal nonvolatile fraction with pigment content, or assume another dispersant has the same solids.
Convert a paste dose into actual pigment
Calculated example: suppose a validated color paste contains 50% dry pigment by mass, and the trial target is 3% dry pigment in 1,000 g finished paint. Required pigment = 1,000 × 0.03 = 30 g; paste = 30 ÷ 0.50 = 60 g; the remaining formula totals 940 g. These are illustrative inputs, not a recommended paste or paint recipe.
That paste also brings 30 g of nonpigment material. Identify its water, resin, dispersant and other carrier components; rebalance the approved formula accordingly. A paste that is 50% total solids is not necessarily 50% pigment. If its pigment fraction is unknown, this calculation cannot be completed reliably.
Mix and track the dispersion
- Clean the vessel and label each trial. Weigh the ingredients and keep an approved control. Record equipment, batch size and material temperature.
- For the specific DISPERBYK-190 route above, homogenize additive with water before gradually adding pigment. Use its current TDS and SDS.
- Disperse using the plant’s suitable laboratory equipment. Sample at repeatable intervals and record grind, viscosity and temperature. Adequate wetting, mechanical breakup and stabilization are separate requirements. Dispersion stages
- Stop at the agreed dispersion endpoint; extra processing time is not automatically better. Let down using the approved sequence, observing any viscosity jump, flocculation or grit.
- Apply equal films to the same substrate and condition them identically. Retain both the concentrated paste and the finished-paint sample.
Check the actual film and stored paint
Compare fineness of dispersion, cured color, tint strength, opacity and gloss. Use the same drawdown thickness, substrate, cure and instrument settings. Include a rub-out check when floating or flooding is suspected. Assess viscosity, settling and redispersibility after the agreed storage exposure. Establish limits from the product specification, not a universal color-difference number. Dose optimization and rub-out checks; Color comparison framework
Troubleshooting before changing color loading
| Observation | Check first | Next controlled action |
|---|---|---|
| Weak or dirty shade | Grind development, base whiteness, film thickness | Repeat one dispersion variable at a time |
| Shade changes after let-down | Paste–binder compatibility | Compare candidate in the actual binder |
| Rubbed area changes shade | Pigment separation or flocculation | Optimize stabilization; repeat full-film test |
| Hard settling or viscosity rise | Storage, surface treatment, additive level | Compare retained paste and complete paint |
Keep an unmodified control so a dispersant improvement is not confused with a different pigment concentration. Poor distribution can affect appearance and flow. Coating defects background
What to send with a sample request
Send FUXIN the dry target panel, binder type, pigment and paste mass balance, A/B/C results, dispersion equipment and process/cure exposure. Include the proposed finish and required QC checks. Ask for a candidate grade supported by current TDS/SDS, then repeat the selected formulation before scale-up.
Technical references
- BYK — DISPERBYK-190 technical data sheet, issue 29 August 2025
- BYK — The dispersion process
- BYK — Practical hints and suggestions
- BYK — Why do we use wetting and dispersing additives?
- ASTM International — ASTM D2244-25: calculation of color tolerances and color differences
Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.