WPC decking and fencing · Practical application guide
WPC Decking & Fencing: A Color Guide
Use a documented composite-color example, then separate full-composite, polymer-only and cap-layer dosage bases.

State which part of the board is colored
Record the polymer family, wood flour, recycled content, additives and whether the colorant goes into the core, the full composite or a coextruded cap. A percentage on the total board is not the same as a percentage on its polymer fraction. The approved board recipe and performance requirements stay in place while color is developed.
For the initial trial, freeze wood source, moisture-conditioning method, resin/recycle lot and surface finish. Otherwise a base-material change can obscure the effect of pigment loading. Coperion treats feeding, compounding and devolatilization as coordinated WPC operations. WPC process controls
A real WPC research example, not a universal oxide dose
Stark and Matuana’s original study used 50% wood flour and compared 1% and 2% Cedar TI-8536, a Holland Colors zinc-ferrite pigment preparation in carrier wax. In the formulations without the UV absorber, HDPE was respectively 49% and 48%. The basis is total composite mass. The study used injection-molded test specimens, not extruded decking; its processing conditions are not a production schedule for your line. This is a named preparation and historical research system, not a FUXIN dry-iron-oxide recipe or a current product guarantee. Original study, Tables 1–2
| Scaled research comparison | Wood flour | Named wax-carried colorant | HDPE | Total |
|---|---|---|---|---|
| Uncolored research control | 5.00 kg | 0 kg | 5.00 kg | 10.00 kg |
| Research colorant level 1% | 5.00 kg | 0.10 kg | 4.90 kg | 10.00 kg |
| Research colorant level 2% | 5.00 kg | 0.20 kg | 4.80 kg | 10.00 kg |
This is arithmetic scaling of selected published formulations, not instructions to run a commercial deck line. The preparation’s dry-pigment fraction is not established here; 2% preparation must not be relabeled 2% pure pigment.
Translate the basis for your own formulation
Calculated comparison: in a hypothetical 10 kg board formula containing 4 kg base polymer, a target of 2% dry pigment on that polymer mass means 80 g pigment. A target of 2% of the 10 kg final composite means 200 g. Those statements differ by a factor of 2.5; write the intended denominator explicitly.
If a compatible concentrate is assumed to contain 40% pigment, supplying 80 g pigment requires 200 g concentrate and brings 120 g carrier/other material. The 40% is an illustration. Use actual composition and have the formulator account for wax, polymer and additives; do not automatically subtract every carrier from the polymer.
Run a finished-profile trial
- Keep the approved control and a documented candidate-loading series. Check the actual pigment/concentrate output from the feeder by weighing delivered material.
- Record wood conditioning and resin/recycled-material identity. Follow the line’s validated moisture and venting controls rather than importing another study’s drying schedule.
- Compound within the approved operating window. Record throughput, material temperatures and process observations; segregate start-up and changeover material.
- Extrude the intended profile using traceable die, cooling and haul-off settings. For capped products, measure and document the actual visible-layer thickness.
- Apply the intended embossing, brushing or sanding before matching. Retain both as-produced and finished specimens when those surfaces differ.
- Sample along the board and across its width, then repeat the chosen formulation with a representative second raw-material lot.
Approve weathering and appearance as a composite
Compare equally conditioned specimens under a fixed measurement method. Mark repeatable locations and surface orientation. Inspect color, texture and surface integrity; carry out the product’s required mechanical and exposure checks. The original study evaluates both appearance and flexural behavior, illustrating why a color reading alone is incomplete. Composite evaluation design
Use an exposure plan relevant to the actual board. Wood, polymer and surface processing contribute to weathering. The pigment’s own stability cannot establish an unfading deck, and accelerated hours do not automatically translate into an outdoor service-life promise. Weathering variables
Troubleshooting table
| Symptom | Check first | Next controlled comparison |
|---|---|---|
| Shade changes despite same pigment lot | Wood/recycle color and feeder records | Fixed-lot reference batch |
| Dark streaks after a stop | Thermal history and changeover material | Stable-run versus restart samples |
| Brushed face is lighter | Wood exposure and brushing settings | Paired as-produced/finished pieces |
| Weathered boards lighten | Whole-composite exposure and surface condition | Matched exposed/unexposed specimens |
Do not add pigment to mask dimensional or mechanical failures. Preserve the approved board construction and evaluate any changed stabilizer or lubricant package independently.
Send the batch ledger with the sample
Provide FUXIN the core/cap route, pigment denominator, concentrate composition, wood/recycle details, process history and finished-board reference. Include the weighed loading series and exposure results so the candidate grade is assessed in the material that customers will actually see.
Technical references
- Stark and Matuana: WPC photostabilizer study, 2006, Tables 1–2
- Coperion — WPC wood plastic composites
- USDA Forest Service, Forest Products Laboratory — Considerations in the weathering of wood-plastic composites
Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.