Request a Quote
Menu ☰

Terrazzo floor · Practical application guide

Cement terrazzo. Color & grinding.

Calculate pigment against the cement matrix and judge it only after the actual chip exposure, filling and polish are complete.

Illustrative pigment application: Terrazzo floor.
Illustrative application image. Confirm the finished shade with physical samples.

Confirm that the matrix is cementitious

This guide concerns cement terrazzo. Epoxy terrazzo uses a resin-controlled formulation and cannot inherit these cement-based ratios. Identify the specified terrazzo assembly, substrate, joints and finishing system before making color samples. The pigment colors the matrix around the chips, so the final result depends on matrix shade, chip selection and how much aggregate grinding reveals.

Use a documented cement-and-chip reference

NTMA’s monolithic-terrazzo guide specification, revised June 2015, gives 94 lb Portland cement per 150 lb marble chips, with pigment if required and enough potable water for workable consistency. This is a reference for that terrazzo system, not a universal recipe for thin overlays or other terrazzo constructions. NTMA mix provisions, page 10

Scaling only those dry proportions gives 10 kg cement plus approximately 15.96 kg chips. Water must follow the selected system and aggregate condition; the reference does not provide a fixed water ratio. Do not invent one from the dry proportions.

Chip-blend calculation exampleFraction of 15.96 kg chipsMass
Chip A60%9.58 kg
Chip B40%6.38 kg
Total100%15.96 kg

The 60:40 combination is a proposed sample blend, not an NTMA color formula. Keep it fixed while evaluating matrix pigment, then change chip proportions in a separate series.

Calculate pigment on the selected binder basis

Suppose the approved pigment candidate is 3% of cement mass. With the 10 kg cement sample, weigh 300 g dry pigment. Do not calculate 3% of cement plus chips: that would give approximately 779 g, a substantially different formulation. Construction-pigment guidance uses defined cementitious denominators, so the recipe must identify which one applies. Pigment dosage context

For a trial comparison, weigh an uncolored control and supplier-approved lower and higher loadings around the selected candidate. Record white or gray cement, chip grading, pigment grade and all actual masses. If you change from gray to white cement for a cleaner pastel, make a new complete sample rather than assuming the previous pigment dose will match.

Cast, grind and fill before approving color

  1. Blend the weighed chips, cement and pigment through the chosen system’s mixing procedure, then add measured water. NTMA’s cited sequence mixes dry components before adding water. Mixing sequence
  2. Cast a labeled sample that can be finished by the intended equipment. Use the planned compaction and curing procedure. Keep enough samples to compare different finishing choices without losing the unmodified reference.
  3. Grind to the specified aggregate exposure. Record the sequence and photograph the surface before filling. A different exposure can appear to be a color change.
  4. Fill pores using the approved matching grout. Calculate its color against its own binder mass; do not assume the main terrazzo’s whole-mix percentage applies. For an already approved 3% binder-based filling recipe, 500 g binder would require 15 g pigment.
  5. Complete the final polish and protective treatment. Mark treated and untreated references so later comparisons remain meaningful.

Evaluate matrix and chip distribution separately

NTMA distinguishes several terrazzo systems and their intended construction. Keep the chosen system’s requirements for thickness, bond and use separate from color approval. System reference

What changedCheck before adjusting pigment
Overall sample looks lighterGreater white-chip exposure or different polish
Small colored fill marksPore-filling grout recipe and finishing
Uneven chip distributionMixing, placement and compaction
Chips pull out during grindingCure readiness and matrix integrity
Sealed sample is darkerTreatment effect on the complete finish

Approve the fully dried, finished sample in the project lighting. Keep the chip blend, matrix recipe and polishing record together; a powder color number alone is insufficient for later repairs. Send FUXIN that record and the preferred sample when requesting a matching pigment grade.

Technical references

Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.

Sample inquiry