Mortar · Practical application guide
Colored mortar.Ratios, trials & mixing.
Start with weighed pigment trials, calculate the correct binder denominator, and use a repeatable mixing and color-checking procedure.

How much pigment should you test?
For an initial dry-powder color comparison, make an uncolored control and 2%, 3% and 4% pigment trials by the declared binder mass. LANXESS Europigments directly recommends 2–4% on cement or lime for its Bayferrox and Oxined powder pigments in concrete or mortar, and advises against exceeding 5% for those products. This supports the trial window below; it does not establish a universal mortar limit or a FUXIN-grade recommendation. Direct concrete-and-mortar powder guidance
Davis’s True-Tone mortar card separately illustrates 1.5%, 3% and 7.5% for most listed colors, against cement or cement plus lime, excluding sand. These differing manufacturer examples show why pigment grade, application and dosage basis must remain identified. The table concerns concentrated dry powder, not carbon black, liquid colorants or filler-diluted packs. Confirm that the selected FUXIN grade permits the proposed trials. Davis mortar examples
Calculate on binder, not the entire mortar bag
Pigment mass = selected percentage ÷ 100 × reference binder mass. For the cement-and-lime basis used here, count the dry cement plus hydrated lime; exclude sand and water. Check the declared basis if supplementary binders are present. Dosage denominator
Each row below is a separate batch with 10.00 kg cement as its only binder. Keep the approved base mortar’s sand, water and additives identical. Pigment is an addition, not a cement replacement.
| Trial | Pigment/binder | Dry powder pigment |
|---|---|---|
| Control | 0% | 0 g |
| A | 2% | 200 g |
| B | 3% | 300 g |
| C | 4% | 400 g |
If the base recipe instead contains 10 kg cement + 2 kg hydrated lime, its reference binder mass is 12 kg: A/B/C require 240/360/480 g. These are calculated examples, not a recommended cement-to-lime ratio. For a small bench mixer, divide every ingredient by ten.
This table does not set cement:sand:water proportions. Keep the mortar type and base recipe already selected for the work. An unknown premixed bag weight cannot supply its binder mass; do not calculate “3%” from the whole bag.
Mix the trial in a repeatable order
- Clean the mixer and label the trial. Weigh pigment rather than measuring scoops. For the 200 g trial, a 5 g weighing error is already 2.5% of the intended pigment addition; use a scale with suitable capacity and resolution.
- One documented mortar sequence is approximately three-quarters of the batch water, then one-third of the sand, then binder and pigment, followed gradually by the remaining sand and water. Solomon specifies at least five minutes to obtain uniform color and workability for its mortar colors. Use this as a reference procedure to verify for the selected grade and mixer. Mortar charging sequence
- Record all water, including aggregate-moisture corrections. Hold batch size and mixing time constant. Do not retemper a stiffening colored batch with extra water. Follow dust controls and wet-cement protection in the material safety sheets.
Choose the base color before increasing dosage
White cement generally produces cleaner, brighter shades; gray cement tends to mute them. Sand color and exposed grains also affect the finish. Make a separate white-cement series when a pale target looks muddy in gray cement. Do not change cement and pigment dosage together during the first comparison. Cement and aggregate effects
Solomon’s dry-concrete sheet reports 7% saturation and warns that over 10% can reduce strength. Its mortar sheet also sets a 10% maximum, including cement plus hydrated lime. These are product-specific limits, not a target dose or proof that every lower dose is safe. If 3% and 4% look nearly alike, compare the extra pigment cost before increasing further. Saturation reference; mortar limitation
Finish and judge dry samples
Make mortar channels or a small panel using the real masonry units and joint profile. Tool the samples at comparable firmness, not merely after equal clock times. Early tooling and overworking can change apparent shade. Cure identically and compare equally dry samples side by side in indirect daylight. Keep the selected sample and make a second independent batch before scaling up. Mortar sample and tooling guidance
Check the process before changing the dose
Troubleshooting before another pigment addition
| What you see | Check first | Next action |
|---|---|---|
| One batch is lighter | Water, sand moisture, binder lot, drying | Repeat with corrected batching records |
| Dark dots or streaks | Clumps, residue, incomplete dispersion | Clean equipment; verify charging and mixing |
| Pale joint edges or dark tooling marks | Finishing firmness and tool pressure | Repeat the joint-finishing trial consistently |
| White surface film | Moisture movement and salt deposits | Investigate the moisture source; trial a compatible cleaner |
Water content, tooling and cleaning can change mortar appearance; aggressive acid cleaning can remove colored surface paste. Test cleaning on a retained panel. Diagnostic background
Technical references
- Solomon Colors: Dry Integral Colors technical specifications (2024), dosage and saturation
- Davis Colors: True-Tone mortar color card, dose examples and binder denominator
- Solomon Colors: SGS Concentrated Mortar Color TDS, limit and mortar mixing method
- Davis Colors: Mortar Color How-To Tips, tooling and color diagnosis
- NPCA: Coloring Precast Concrete, cement and aggregate color effects
- Davis Colors: Product data, mineral pigments and carbon-black distinction
- LANXESS Europigments: Bayferrox and Oxined powder instructions for concrete and mortar
Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.
Turn your trial into a sample request
Before production, check the selected mortar against its required workability and hardened-performance criteria. Send FUXIN the preferred dry sample, binder recipe and A/B/C results to request the matching grade and supply quotation.