Iron Oxide Brown
Request a QuoteFUXIN pigment range
Iron Oxide Brown
Brown pigment for specification enquiries, with four documented grade references and a cement application reference price.
per metric tonne
Select an application to see the relevant quotation information.
Compare Brown 610, 841, 663 and 686. Brown and Ochre remain separate product enquiries.
Request a QuoteFour references within the brown family.
Brown 610, 841, 663 and 686 are documented separately. Choose a reference to start your shade comparison, and confirm the relevant specification for the material you plan to color.
Discuss your applicationProduct at a glance
- Product family
- Iron Oxide Brown
- Documented grade references
- 610 · 841 · 663 · 686
- Application enquiry
- Cement
- Product selection
- Confirm grade, shade and material system
Compare Brown 610, 841, 663 and 686. Brown and Ochre remain separate product enquiries.
Grade reference data
Compare the documented references below. Brochure values are provided for initial selection; confirm the current grade specification and test methods before ordering. These values do not establish asphalt suitability.
| Grade reference | Oil absorption ml/100 g | pH | 325-mesh residue % | Moisture % | Tamped apparent density g/cm³ |
|---|---|---|---|---|---|
| 610 | 20–30 | 4–7 | ≤0.3 | ≤1.0 | 0.7–1.1 |
| 841 | 20–30 | 4–7 | ≤0.3 | ≤1.0 | 0.7–1.1 |
| 663 | 20–30 | 4–7 | ≤0.4 | ≤1.0 | 0.8–1.2 |
| 686 | 20–30 | 4–7 | ≤0.3 | ≤1.0 | 0.8–1.2 |
Source: product brochure, technical specification table, page 4. Tamped apparent density is not true density. Missing values are not inferred.
Ask for the current data sheet for your selected grade and application.
Request grade-specific TDS →Application guidance
Confirm the pigment system against your material, target shade and process conditions.

Cement-based materials
Compare a Brown grade in the intended cement or concrete mixture. Tell us your shade reference, mixing process and approximate quantity.
Request the relevant technical data sheet
Include the product family and application so the response is specific to your enquiry.
Helpful details for your request
- Iron Oxide Brown and preferred grade, if known
- Application and material system
- Target shade and reference sample
- Process conditions and approximate quantity
Where brown takes shape.
Application imagery is a general example, not a verified shade or grade reference.

Cement-based materials
Compare a Brown grade in the intended cement or concrete mixture. Tell us your shade reference, mixing process and approximate quantity.
Application images are illustrative. Actual color depends on the material system and process.
Need brown specifications?
Share your application, preferred grade and target shade.