Artificial marble · Practical application guide

Cement-based marble. Color & polishing.

Calculate background and vein pigment separately, then compare patterns after the real polishing and sealing process.

Illustrative pigment application: Artificial marble.
Illustrative application image. Confirm the finished shade with physical samples.

Confirm whether the binder is cement or resin

Artificial marble can describe different manufactured materials. This page concerns cement-bound decorative slabs and cast objects. Polyester, epoxy and other resin-bound products need a separate pigment-compatibility and cure assessment. Identify the binder before ordering samples. Define whether the desired appearance is a smooth colored matrix, exposed chips, a vein pattern, or a combination; each needs its own approval specimen.

Make a background-color ladder first

For the first background screen, use an uncolored control plus 1%, 2% and 4% dry-pigment candidates only if permitted for the selected grade. The Concrete Countertop Institute describes 0.5–5% of total cementitious mass as typical in its countertop context. The nonzero pigment levels are within that reference interval; it is not a recipe for resin-bound marble or a FUXIN limit. Range and material context

Keep decorative chips and veins out of this first decision. Select the background on a cured, processed specimen, then introduce the pattern as a separate variable. This prevents a stronger vein or brighter chip blend from disguising an unsuitable base shade.

Calculate the two cementitious mixes independently

Use pigment = declared cementitious mass × percentage ÷ 100. The table is arithmetic for separate qualified mixes, with no prescribed cement:sand:water proportions.

Mix componentReference binder1% pigment2% pigment4% pigment
Background trial2.00 kg20 g40 g80 g
Small vein trial0.50 kg5 g10 g20 g
Larger background10.00 kg100 g200 g400 g

If the selected background is 2% and the selected vein is 4%, the first two rows require 40 g and 20 g respectively. Do not calculate the vein pigment from the whole slab’s binder. Do not assume a dark vein uses the same dosage as the background; approve each dry color first. Fine pigment doses need an appropriately accurate scale.

Cast a repeatable pattern experiment

  1. Prepare separately identified background and vein batches. Record each mixture’s water and admixture quantities as well as pigment.
  2. Use the same mould and filling direction. Weigh the amount of ready-mixed accent material used, and photograph where it is placed.
  3. Change one pattern variable per specimen: accent amount, placement path, or the number of combining passes. Keep the two qualified material recipes unchanged during this aesthetic comparison.
  4. Record the time between preparing the mixes and combining them. Avoid uncontrolled extra water to stretch a stiffening vein batch.
  5. Cast a plain companion and a patterned specimen from each run. Keep a repeat pattern made independently to assess reproducibility, not just a one-off attractive effect.

Polish before approving the pattern

Record the finishing machine, abrasive sequence and the point at which the target exposure is reached. Compare an as-cast companion, a processed piece and a sealed piece. The Countertop Institute notes that a smooth color sample does not automatically represent exposed-aggregate finishes. Sample and finish distinction

Inspect the edge and a cut section as well as the centre. Confirm that the vein remains visible where machining removes material. If different mixtures meet at an interface, the fabricator must verify that the finished composite is sound; an attractive pattern is not evidence of adequate bond or flexural performance.

Symptoms, likely causes and next trials

SymptomCheck firstNext action
Vein disappears after polishingPattern depth and removalRepeat the pattern/finishing trial together
Broad muddy colorToo much intermixing or unsuitable backgroundReduce combining action; keep pigment fixed
Dark isolated spotsPigment incorporationMake a plain dispersion control
Crack or open interfaceDifferent mixtures and casting intervalStop; evaluate compatibility and process
Repair stands outGrout texture, color and finishApprove repair on a spare processed sample

Keep a formula and photograph for each candidate rather than an informal instruction such as add a little black. A change in aggregate exposure can shift the apparent shade even when pigment is unchanged. Aggregate-exposure background

Scale the approved result

Repeat at a larger pattern scale before committing to full panels. Preserve background/vein mass ratios, placement sequence and processing records while the fabricator confirms the production method. Complete the intended end-use tests for the entire finished system. Send FUXIN the preferred dry samples, both weighed color formulas and photographs before and after processing; that evidence is more useful than one polished hero image.

Technical references