Fiber cement boards · Practical application guide
Fiber Cement Boards: Pigment Mass Balance
Calculate body pigment and slurry carrier water, then verify the color through sheet formation, pressing and the real cure.

Define through-color and surface color separately
Decide whether the board needs a colored body, a colored surface coating, or both. Swisspearl’s production overview describes through-color introduced during slurry production and separate applied surface finishes. A pigment approved for one route is not automatically suitable for the other. Confirm the intended board process, fiber system, cure route and finish with the manufacturer before selecting candidate grades. Swisspearl: Fiber Cement Production
Set the dosage basis before the line trial
The cited board manufacturers describe pigment in the slurry but do not publish a universal pigment-loading range for all fiber-cement recipes. Use the board system’s qualified loading. The 1%, 2% and 3% columns below are conversion examples, not an instruction to run an unapproved dose or autoclave cycle.
State whether the plant formula expresses pigment against cement, a defined cementitious fraction, or all dry feed. Do not include quartz filler, cellulose or process water in a cement-only denominator. EQUITONE describes a specific slurry-forming, dewatering, pressing and autoclaving route; that process must be evaluated as a whole. Documented board process
Use a clear pilot-batch mass table
| Declared reference mass | 1% dry pigment | 2% dry pigment | 3% dry pigment |
|---|---|---|---|
| 5 kg | 50 g | 100 g | 150 g |
| 20 kg | 200 g | 400 g | 600 g |
| 100 kg | 1,000 g | 2,000 g | 3,000 g |
For a hypothetical pilot with 20 kg cement and 50 kg total dry feed, 400 g pigment is 2% of cement and 0.8% of the original dry feed. Record both values only with their names. This is a denominator illustration, not a board composition recommendation. Pigment addition changes the total feed mass, so the production mass balance must use a consistent convention.
If that 400 g dry-pigment target is supplied as a verified 50%-pigment, 50%-water dispersion, weigh 800 g dispersion and account for 400 g water. Real suspension composition must be confirmed; total solids need not equal pigment solids.
Trace the trial through the line
- Identify the baseline recipe, pigment lot, approved dosing point and trial start/finish. Re-homogenize a supplied slurry using its instructions.
- Record the actual pigment and carrier masses, slurry solids measurement, mixer/agitator settings and delay before forming.
- Sample the feed and identify sheets at the start, middle and end of the run. Note any preceding color and the changeover method.
- Carry the trial through the actual sheet-forming/dewatering route, pressing, cure and finishing. Keep those settings linked to the sheet identifiers.
- Where process water recirculates, track its state during changeover and involve the plant technologist in the pigment-retention and carry-over assessment. A sample taken from fresh slurry alone cannot establish steady production behavior.
Use a board-specific inspection grid
| Location/condition | Check | Record |
|---|---|---|
| Start, middle, end sheets | Run-to-run color drift | Sheet ID and production time |
| Centre versus edges | Streaking or forming variation | Marked photo positions |
| Face versus machined section | Body color and layer appearance | Surface treatment and cut position |
| After actual cure | Color change and board quality | Full curing record |
| After sanding/coating | Final hue, sheen and pattern | Finish recipe and direction |
Swisspearl distinguishes through-color from applied surface color. Keep the two evaluations separate. Body versus surface finish For autoclaved boards, a pigment that looks acceptable after room-temperature curing has not yet passed the required process trial.
Diagnose before increasing pigment
| Symptom | Likely investigation | Action |
|---|---|---|
| Shade drifts during the run | Feed consistency or recirculated process water | Check time-linked samples and mass balance |
| Lines follow machine direction | Forming or finishing stage | Compare unprocessed and finished sheets |
| Change appears only after cure | Cure cycle or pigment-system suitability | Hold recipe and investigate actual-cycle compatibility |
| Cut edge differs from coated face | Different color routes | Assess against the specified body/face design |
EQUITONE notes that light and moisture influence appearance, so compare similarly conditioned boards in a defined orientation. Appearance conditions Do not use another brand’s tolerance as the acceptance limit for your board.
Release the complete panel formulation
Repeat the selected pilot under production conditions and verify the board’s required mechanical, moisture and durability properties. Retain representative sheets and all feed/cure/finish records. Send FUXIN the selected pigment mass basis, slurry and carrier composition, forming route, actual thermal cycle and final board samples; those details allow a focused grade assessment without substituting a generic concrete recipe.
Technical references
- Swisspearl: Fiber Cement Production
- EQUITONE: Tectiva Material Information
- LANXESS Europigments: Product-use guidance
Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.