Resin crafts · Practical application guide
Resin Crafts: Mixing & Casting Guide
Use a documented resin-specific example to understand the dose basis, then preserve the resin’s required mixing ratio while testing color.

Choose the resin and the colorant together
Identify epoxy, polyurethane or another casting chemistry before selecting powder or paste. Confirm the selected pigment’s chemistry and the paste carrier, if any. Keep a clean mold, suitable balance and labeled control casting ready. Follow the resin and pigment SDS for ventilation, skin/eye protection and handling. The example below is an industrial casting-resin reference, not an endorsement for children’s activities or a general household craft recipe.
A reactive resin’s A/B ratio determines its cure chemistry. Colorant does not replace either component. Do not add extra hardener to compensate for pigment, to accelerate a cure, or to make a tacky casting acceptable. Epoxy cure troubleshooting
A real manufacturer dose and mix-ratio example
Smooth-On’s Smooth-Cast 325 instructions give 0.5–1% of its specified colorant by Part B mass as a color example. The resin ratio is 115 A : 100 B by mass, distinct from 1 A : 1 B by volume. Its instructions put colorant into Part B before combining the components. These figures apply to that resin and its indicated compatible colorants, not directly to loose FUXIN pigment or an epoxy. Smooth-Cast 325 source instructions
The table is a scaled weighing example using those instructions. The middle color level is an interpolated comparison, not a separate manufacturer recommendation.
| Trial | Neat Part A | Neat Part B | Colorant/Part B | Colorant | Combined mass |
|---|---|---|---|---|---|
| Control | 115 g | 100 g | 0% | 0 g | 215 g |
| A | 115 g | 100 g | 0.50% | 0.50 g | 215.50 g |
| B | 115 g | 100 g | 0.75% | 0.75 g | 215.75 g |
| C | 115 g | 100 g | 1.00% | 1.00 g | 216.00 g |
Calculated from colorant mass = neat B mass × dose fraction. Use the mass of B before pigment addition. Do not weigh A to match the increased mass of colored B.
Do not mistake colorant paste for pure pigment
If the 1.00 g colorant in that example were documented as 40% pigment, it would deliver 0.40 g dry pigment; in 216.00 g combined material that is 0.185% pigment. The 40% value is a calculation assumption, not a claim about Smooth-On’s products. The remainder is carrier or other ingredients whose compatibility also matters.
For a dry-powder candidate, do not substitute the same supplied mass and assume equivalence. Match an agreed active-pigment target only after reviewing chemistry, dispersion and resin effects. If a paste contains reactive carrier resin, have the formulation owner account for its functionality; a simple solids conversion cannot establish chemical equivalence.
Use the addition sequence for your actual system
- Weigh neat resin components separately, then the approved colorant. Record material lots, room/material conditions and mold geometry.
- For the Smooth-Cast example, uniformly preblend colorant into B, then combine with the correctly measured A and mix as instructed. For WEST SYSTEM epoxy, the documented route instead mixes resin and hardener thoroughly before additives. These sequences are not interchangeable. WEST SYSTEM sequence
- Scrape the container sides and bottom during mixing without introducing unnecessary air. Prepare a control with the same handling.
- Cast within the specified pot life, batch-mass and pour-depth limits. A thin trial does not justify pouring a deeper or much larger mass; reactive resins can generate substantial heat.
- Condition each casting for the specified full cure before assessing its color or hardness. Label the top, bottom and any cut section.
Examine color, settling and cured quality
Compare castings at equal thickness, on the same backing and under consistent light. Inspect the underside for sediment concentration and a cut surface for unmixed streaks. Check tackiness, soft areas, bubbles and demolding damage. Apply the intended sanding, polishing or topcoat to a companion specimen. Keep a neat control to identify whether the base resin is itself producing a defect.
For exposure-sensitive objects, test the complete resin/finish system. A stable pigment cannot prevent every resin color change. WEST SYSTEM separately specifies UV protection for its pigmented epoxy applications. Pigmented epoxy finish guidance
Troubleshooting table
| Symptom | Checks | Next action |
|---|---|---|
| Tacky or soft casting | A/B basis, mixing, colorant compatibility | Reject/review against the control; do not add hardener |
| Foaming in polyurethane | Moisture in ingredients, tools or storage | Repeat with compliant dry materials |
| Dark bottom / light top | Settling and working time | Review pigment form and suspension |
| Correct wet shade, wrong cured shade | Thickness, cure and base-resin color | Match the fully cured geometry |
Overloading or using an incompatible color system can interfere with cure. Colorant compatibility warning
Request the right sample
Send FUXIN the resin grade, A/B basis, proposed colorant form, target opacity, pour geometry and measured trial results. Request a candidate for that resin and keep the final approved mixing sheet with the cured reference casting.
Technical references
- Smooth-On — Smooth-Cast 325 technical product guidance
- WEST SYSTEM — Epoxy problem solver
- Smooth-On — How can I add color to liquid rubber or liquid plastics?
- WEST SYSTEM — 502 black pigment
Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.