Self-leveling mortar · Practical application guide
Self-leveling mortar. Color & compatibility.
Use current additive permission and an explicit dosage denominator before introducing color into a balanced self-leveling formulation.

Get current written permission before weighing pigment
First distinguish a wearing topping from an underlayment intended to be covered. Coloring an underlayment does not make it a finished floor. For any packaged self-leveling product, identify the current technical sheet and obtain written permission for the exact pigment, quantity and incorporation method. Do not rely on an old guide specification to authorize an additive.
ARDEX PC-T’s September 2026 TDS states that additives outside its written recommendations must not be mixed in. This TDS supersedes its earlier versions. Accordingly, no historical pigment allowance is used as permission or as a trial limit in this guide. Current PC-T technical sheet A FUXIN pigment suitable for ordinary cement is not automatically approved for a proprietary topping.
Calculate only the loading already authorized for your system
The following is an independent arithmetic example for a different, hypothetical system whose manufacturer has expressly approved 1% on total dry powder. It is not an ARDEX PC-T recipe and does not recommend 1% for an untested self-leveling product.
| What the written approval specifies | Reference mass | Calculation |
|---|---|---|
| 1% of all dry topping powder | 10 kg | 100 g pigment |
| 1% of binder only, if separately specified | 3 kg binder within that powder | 30 g pigment |
These bases cannot be exchanged. Confirm whether pigment is an addition or replaces a named ingredient, and whether its form is dry powder or a preparation containing water. Keep the approval with the batch sheet. If no approved dose exists, collect compatibility samples and technical information without proceeding to a floor installation.
Keep the unmodified product’s mixing data separate
For its standard, unmodified product route, the current PC-T sheet lists 5 US quarts, approximately 4.75 L, per 50 lb bag. Its manual method mixes two bags at a time for approximately 2–3 minutes; the corresponding standard water quantity is approximately 9.5 L. These are product-specific baseline instructions, not permission to add pigment or water. Current water and mixing data
In an expressly approved pigmented system, use that system’s agreed water calculation and mixing method. Record powder, pigment, water, temperature and elapsed time separately. A smaller spread after pigment addition is useful test information; adding water to hide it would change the experiment and may weaken the material.
Make the comparison measurable
Before starting, write a one-page trial sheet. Include the approved base, pigment identity, dose basis, batch size, water quantity, test method and acceptance criteria. Prepare an unmodified control alongside the permitted candidate. Use the product’s specified flow test at the same elapsed time for both; do not invent an acceptable spread diameter.
Repeat the approved candidate independently. One successful cup can miss weighing error or incomplete dispersion. Note foam, lumps, settling, surface skinning and any change in the useful placement window. If the flow or working behavior fails, stop the trial rather than adjusting the water or additives without approval.
Carry the trial through the finished-floor process
- Reproduce the specified substrate preparation, moisture control and primer in a representative bay. An unprimed board cannot establish floor adhesion.
- Mix and place the authorized formulation at its permitted thickness. Keep the actual charging and placement times with each sample.
- Include a batch junction and use the intended spreading and smoothing tools. Preserve the floor design’s joints.
- Follow the specified drying, grinding, polishing and sealing route. Record the finishing stage used for each comparison.
- Compare equally dry finished samples and complete the required bond, strength and wear checks before production release.
Use differences to choose the next action
| Observation | Check first |
|---|---|
| Lower flow | Water measurement, pigment compatibility, test timing |
| Foam or settling | Mixing and water control |
| Visible batch boundary | Placement timing and consistency |
| Pinholes | Substrate preparation and entrained air |
| Color changes after polish | Grinding depth and protective treatment |
Do not treat a change in gloss as proof of a different pigment dose. Retain the control, finished sample and written approval together. Send FUXIN the permitted formulation basis and trial observations for grade selection; the topping manufacturer remains the source of permission for external colorant addition.
Technical references