Colored pavement · Practical application guide

Colored concrete pavers. Face-mix trials.

Calculate pigment only against the relevant colored layer, then approve both individual pavers and the laid color distribution.

Illustrative red and charcoal concrete paving blocks beside a landscaped planter.
Illustrative application image. Confirm the finished shade with physical samples.

Identify the layer that needs pigment

A concrete paver may be colored throughout or have a separately manufactured colored face layer. Obtain the actual product cross-section and batch sheet. Pigment for a face mix is calculated against that face mix’s specified binder basis, not automatically against cement in the backing layer. The product’s required face thickness and performance remain part of the existing design.

Use an application-specific starting reference

MAPEI’s Color Paving Pigment sheet gives 3–6% on cement with gray cement, and 1–4% with white cement for its product range. These are named-product references for selecting trial levels, not FUXIN dosage guarantees. It also notes that greater pigment addition eventually gives little extra color. Concrete-paving dosage guidance

For a gray-cement face mix with 20 kg cement, an initial supplier-approved comparison at 3%, 4% and 5% would require:

Face-mix samplePigment / cementDry powder
Control0%0 g
A3%600 g
B4%800 g
C5%1,000 g

Keep sand, water and additives unchanged during this comparison. If a product instead declares total cementitious mass as its basis, recalculate accordingly. The selected pigment grade and complete paver formulation determine which levels may be tested.

Avoid a face-layer budgeting error

Suppose a production allocation contains 20 kg face-layer cement plus 40 kg backing-layer cement. At the selected 4% face-cement dose, pigment is 0.8 kg. Calculating 4% of all 60 kg would produce 2.4 kg, triple the intended face-mix addition.

Keep face and backing records separate even if one production controller manages both. Do not save pigment by making an unapproved thinner face layer. That changes the product rather than merely its color. For full-depth color, use the complete colored mix’s approved reference binder and reassess the sample.

Run the press or casting trial

  1. Check pigment metering and aggregate moisture. Identify the incoming cement and pigment lots.
  2. Use the validated charging sequence and mixer fill level. Inspect a smear or pressed sample for dispersion before assuming more pigment is needed.
  3. Form on the production equipment, recording vibration, compaction and face-feed settings. Davis’s manufacturing guidance identifies these as variables affecting surface appearance. Manufactured-unit process controls
  4. Label samples from different positions in the run and curing area. Complete the normal curing, finishing and packaging route.
  5. Compare dry units under the same light, then complete the required dimensions, strength, wear and exposure checks. Keep those results beside the appearance approval.

Approve the laid blend, not one attractive paver

For a proposed two-color layout with 70% color A and 30% color B, a 100-unit sample needs 70 A and 30 B units. This is a design-distribution example, not a pigment blend inside the mixer. Lay them using the intended pattern and distribution method. A pile of correctly colored units can still produce an unwanted banded installation.

Record the accepted blend with a photograph and unit identities. Evaluate the display dry and wet. Retain replacement samples from each component color so later orders can be matched to their individual formulas.

Troubleshoot the visible surface

AppearanceCheck first
Pale hazeDeposits and moisture history
Vertical bands in the layoutUnit distribution and batch grouping
Rougher units look darkerCompaction and surface texture
Color changes after wearAggregate exposure and cement-paste loss
One batch is off-shadeWeighing, binder and water records

CMHA’s maintenance guidance distinguishes efflorescence and surface changes from pigment fading. Paver appearance and maintenance Test any cleaner or sealer on retained units. Send FUXIN the face/full-depth route, cement basis, desired dry sample and manufacturing results when requesting a pigment grade.

Technical references

Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.

Sample inquiry