Resin-bound paving · Practical application guide
Resin-bound paving. Aggregate & color trials.
Keep aggregate blending, resin-component ratio and any authorized pigment addition as three separate calculations.

Confirm the system and where its color comes from
Resin-bound paving mixes aggregate and binder before placement. Resin-bonded surfacing broadcasts aggregate onto a resin layer and uses a different process. Identify the selected system before buying materials. In many resin-bound surfaces, stone color and the resin’s appearance provide the desired shade without extra pigment.
SureSet explains that non-UV-resistant resin can change the apparent aggregate color under sunlight. Select the binder and aggregate together. Do not try to correct an unsuitable resin choice by adding iron oxide on site. Resin and appearance guidance
Calculate the aggregate blend first
For a proposed 60:40 blend of two approved aggregates, a 25 kg sample batch contains 15 kg aggregate A and 10 kg aggregate B. A 100 kg material plan contains 60 kg and 40 kg respectively. This visual blend ratio does not set the resin quantity.
Keep the approved particle sizes and any specified sand unchanged. More fine material can alter the finished surface, so do not add arbitrary sand to make a mix easier to trowel. Evaluate the bonded sample after curing rather than approving only loose aggregate in a bag.
Use pigment only under formulation-specific permission
For a manufacturer developing a pigmented binder, obtain approval for pigment chemistry, moisture, dispersion route and the precise dose basis. No universal FUXIN powder percentage or resin-to-aggregate ratio is offered here.
The following is independent arithmetic for a hypothetical system that already permits 1% pigment on combined resin mass:
| Reference being used | Mass | Result at 1% |
|---|---|---|
| Approved combined resin components | 2.0 kg | 20 g pigment |
| Resin plus 25 kg aggregate, incorrectly substituted as the basis | 27.0 kg | 270 g pigment |
The incorrect denominator gives 13.5 times the intended amount. The 2 kg resin figure is not a recommended binder content for 25 kg aggregate. Maintain the manufacturer’s exact component ratio; adding more hardener to compensate for pigment is not an acceptable calculation. If no external pigment is permitted, use the approved aggregate/color system instead.
Make a cured comparison with controlled mixing
- Confirm the material storage, aggregate dryness and ambient conditions required by the system. Keep a record of component and aggregate lots.
- Mix the complete resin components in their prescribed proportions and sequence. Avoid partial kits unless the manufacturer provides an accurate weighing method.
- Incorporate any specifically authorized pigment at the approved stage. Mix the aggregate and resin until coating is uniform, then add only the system’s prescribed remaining components.
- Record mixing time and repeat it for later batches. SureSet’s installation guidance emphasizes uniform coating and consistent cycles; its directions are for its complete kit, not permission for additional pigment. Mixing process reference
- Place the sample at the system’s specified depth, reproduce the intended finishing and allow the required cure. Include a batch junction and an identified unpigmented reference when testing a new binder formulation.
Inspect function as well as shade
Compare dry color, gloss and aggregate distribution. Look for soft spots, foaming, loose stone and excess binder at the surface. Confirm the finished system’s required bond, wear, slip and drainage properties. A pigment or fine-material change requires renewed assessment rather than an assumption of unchanged permeability.
| Problem | Check before changing pigment |
|---|---|
| Yellowing | Resin exposure suitability |
| Foam or whitening | Moisture and mixing conditions |
| Loose aggregate | Binder coverage and cure |
| Dark trowel marks | Overworking and finishing method |
| Slower water entry | Surface closing and full build-up |
Do not apply a remedial sealer before investigating its effect on the surface and drainage. Keep the cured reference, approved formula and batch records together. Send FUXIN the resin chemistry, permitted addition basis and trial findings for manufacturer-led grade selection; an installer should obtain the complete-system supplier’s authorization before any external pigment addition.
Technical references
- SureSet: Resin types and appearance
- SureSet: Complete resin-bound kit mixing example
- SureSet: Specification and maintenance documents
Independent technical guidance used for this application overview. These references are not FUXIN project case studies or a substitute for a grade-specific technical data sheet.